MIL-DTL-2710C
TABLE V. First article examination and tests - Continued.
Requirement
Examination or test
Inspection
paragraph
paragraph
C-link component
Chemical composition
3.2.1.1
4.5.1
Tensile test
3.4
4.5.4
Pull draft angle
3.7.1
4.4.1.1
Brinell hardness test 1
3.5
4.5.6
Dimension conformance
3.7
4.4.1
Surface
3.8
4.4.2
Markings
3.15, 3.15.1
4.4.4
Identification numbers
3.16
4.4.5
Right and left hand coupling plates
Chemical composition
3.2.1.1
4.5.1
Tensile test
3.4
4.5.4
Pull draft angle
3.7.1
4.4.1.1
Brinell hardness test 1
3.5
4.5.6
Dimension conformance
3.7
4.4.1
Surface
3.8
4.4.2
Markings (right hand coupling plate only)
3.15
4.4.4
Identification numbers
3.16
4.4.5
Fit
3.10
4.4.6
Taper pin
Chemical composition
3.2.2.1
4.5.1
Brinell hardness test 1
3.6
4.5.5
Dimension conformance
3.7
4.4.1
Surface
3.9
4.4.3
Engagement
3.11
4.4.7
Plug
Chemical composition
3.2.3.1
4.5.1
Dimension conformance
3.7
4.4.1
Hairpin (when specified (see 6.2))
Chemical composition
3.2.4.1
4.5.1
Dimension conformance
3.7
4.4.1
Fit
3.12
4.4.8
¹ Hardness measurement methods, tests and testers such as Rockwell, Knoop, and Vickers, shall be direct
equivalents to Brinell and may be substituted solely in accordance with ASTM A370 (see 6.4).
4.2.1 First article inspection samples. The following samples shall be prepared for first
article inspection examinations and tests specified in table V. Samples shall be clean, bright, and
free of paint or other coatings which would tend to conceal defects during inspection or testing.
Detachable link samples shall consist of a minimum of:
10